El propósito de este estudio preliminar es evaluar el push-out bond strength de los postes de dentina experimentales (PDE) obtenidos de dientes humanos y bovinos esterilizados por autoclave y radiación gamma. Ochenta y cuatro premolares mandibulares fueron obturadores y se dividieron en tres grupos...

Descripción completa

Detalles Bibliográficos
Autores principales: Tulga DDS, PhD, Ayça, Ayşe Şanal DDS, PhD, Fatma, Ömür Dede DDS, PhD, Doğu
Formato: Online
Idioma:eng
Publicado: Universidad de Costa Rica 2019
Acceso en línea:https://revistas.ucr.ac.cr/index.php/Odontos/article/view/36506
id ODONTOS36506
record_format ojs
institution Universidad de Costa Rica
collection Odovtos International Journal of Dental Sciences
language eng
format Online
author Tulga DDS, PhD, Ayça
Ayşe Şanal DDS, PhD, Fatma
Ömür Dede DDS, PhD, Doğu
spellingShingle Tulga DDS, PhD, Ayça
Ayşe Şanal DDS, PhD, Fatma
Ömür Dede DDS, PhD, Doğu
Does Sterilization Affect the Push Out Bond Strength of Experimental Dentin Posts?
author_facet Tulga DDS, PhD, Ayça
Ayşe Şanal DDS, PhD, Fatma
Ömür Dede DDS, PhD, Doğu
author_sort Tulga DDS, PhD, Ayça
description El propósito de este estudio preliminar es evaluar el push-out bond strength de los postes de dentina experimentales (PDE) obtenidos de dientes humanos y bovinos esterilizados por autoclave y radiación gamma. Ochenta y cuatro premolares mandibulares fueron obturadores y se dividieron en tres grupos experimentales de postes: el grupo de fibra de vidrio (Fb) grupo PDE humano (Hm) y el grupo PDE bovino (Bv). Se obtuvieron tres subgrupos (n=12) para cada grupo de PDE según los métodos de esterilización; sin esterilización (Cnt), autoclave a vapor (Aut) y radiación gamma (Rad) con una dosis total de 25 kGy. Todos los postes se cementaron a los conductos radiculares utilizando un cemento de resina de curado doble (Panavia SA). Después de que se obtuvieron las micro rebanadas (1 mm de espesor) de cada subgrupo, se realizó una prueba de push-out bond strength. Los datos se analizaron utilizando ANOVA de dos vías y las pruebas de comparación múltiple de Tukey (α=.05). El tipo de poste y el método de esterilización fueron significativamente efectivos en los valores de push-out bond strength según el ANOVA (P <.001). Los grupos de PDE no aplicados a la esterilización mostraron valores de push-out bond strength significativamente mayores que los grupos esterilizados (p <0,001). Bv_Cnt (9.42 ±1.31) mostró valores de push-out bond strength significativamente más bajos que los grupos Fb (12.36 ±1.54) y Hm_Cnt (11.06 ±1.38) (P <.001). Tanto el autoclave al vapor como la radiación gamma afectan negativamente los valores de push-out bond strength y los modos de fractura de los PDE. Los PDE bovinos no son tan efectivos como los PDE humanos con respecto a la fuerza de adhesión a la dentina de la raíz.
title Does Sterilization Affect the Push Out Bond Strength of Experimental Dentin Posts?
title_short Does Sterilization Affect the Push Out Bond Strength of Experimental Dentin Posts?
title_full Does Sterilization Affect the Push Out Bond Strength of Experimental Dentin Posts?
title_fullStr Does Sterilization Affect the Push Out Bond Strength of Experimental Dentin Posts?
title_full_unstemmed Does Sterilization Affect the Push Out Bond Strength of Experimental Dentin Posts?
title_sort does sterilization affect the push out bond strength of experimental dentin posts?
publisher Universidad de Costa Rica
publishDate 2019
url https://revistas.ucr.ac.cr/index.php/Odontos/article/view/36506
work_keys_str_mv AT tulgaddsphdayca doessterilizationaffectthepushoutbondstrengthofexperimentaldentinposts
AT aysesanalddsphdfatma doessterilizationaffectthepushoutbondstrengthofexperimentaldentinposts
AT omurdededdsphddogu doessterilizationaffectthepushoutbondstrengthofexperimentaldentinposts
_version_ 1810113431615832064
spelling ODONTOS365062021-06-09T22:03:17Z Does Sterilization Affect the Push Out Bond Strength of Experimental Dentin Posts? Tulga DDS, PhD, Ayça Ayşe Şanal DDS, PhD, Fatma Ömür Dede DDS, PhD, Doğu Dentin post; Gamma radiation; Steam autoclaving; Push-out bond strength Poste de dentina; Radiación de gama; Autoclave al vapor; Push-out bond strength The purpose of this preliminary study is to evaluate the push-out bond strength (PBS) of experimental dentin posts (EDPs) obtained from human and bovine teeth sterilized by autoclaving and gamma radiation. Eighty-four mandibulary premolars were obturated and divided into three post groups: the glass fiber group (Fb) human EDP group (Hm) and the bovine EDP group (Bv). Three subgroups (n=12) were obtained for each EDP groups according to the sterilization methods; no sterilization (Cnt), steam autoclaving (Aut), and gamma radiation (Rad) a total dose of 25 kGy. All posts were cemented to root canals using a dual cured resin cement (Panavia SA). After the micro slices (1mm in thickness) were obtained of each subgroup, PBS test was performed. Data were analyzed using two-way ANOVA and Tukey’s multiple comparison tests (α=.05). The post type and sterilization method was significantly effective on the PBS values according to the ANOVA (P<.001). No sterilization apllied EDP groups showed significantly higher PBS values than the sterilized groups (P<.001). Bv_Cnt (9.42 ±1.31) showed significantly lower PBS values than both Fb (12.36 ±1.54) and Hm_Cnt (11.06 ±1.38) groups (P<.001). Both steam autoclaving and gamma radiation affect the PBS values and fracture modes of EDPs negatively. The bovine EDPs are not as effective as human EDPs with regard to the PBS to the root dentin. El propósito de este estudio preliminar es evaluar el push-out bond strength de los postes de dentina experimentales (PDE) obtenidos de dientes humanos y bovinos esterilizados por autoclave y radiación gamma. Ochenta y cuatro premolares mandibulares fueron obturadores y se dividieron en tres grupos experimentales de postes: el grupo de fibra de vidrio (Fb) grupo PDE humano (Hm) y el grupo PDE bovino (Bv). Se obtuvieron tres subgrupos (n=12) para cada grupo de PDE según los métodos de esterilización; sin esterilización (Cnt), autoclave a vapor (Aut) y radiación gamma (Rad) con una dosis total de 25 kGy. Todos los postes se cementaron a los conductos radiculares utilizando un cemento de resina de curado doble (Panavia SA). Después de que se obtuvieron las micro rebanadas (1 mm de espesor) de cada subgrupo, se realizó una prueba de push-out bond strength. Los datos se analizaron utilizando ANOVA de dos vías y las pruebas de comparación múltiple de Tukey (α=.05). El tipo de poste y el método de esterilización fueron significativamente efectivos en los valores de push-out bond strength según el ANOVA (P <.001). Los grupos de PDE no aplicados a la esterilización mostraron valores de push-out bond strength significativamente mayores que los grupos esterilizados (p <0,001). Bv_Cnt (9.42 ±1.31) mostró valores de push-out bond strength significativamente más bajos que los grupos Fb (12.36 ±1.54) y Hm_Cnt (11.06 ±1.38) (P <.001). Tanto el autoclave al vapor como la radiación gamma afectan negativamente los valores de push-out bond strength y los modos de fractura de los PDE. Los PDE bovinos no son tan efectivos como los PDE humanos con respecto a la fuerza de adhesión a la dentina de la raíz. Universidad de Costa Rica 2019-03-12 info:eu-repo/semantics/article info:eu-repo/semantics/publishedVersion Article application/pdf text/html application/epub+zip https://revistas.ucr.ac.cr/index.php/Odontos/article/view/36506 10.15517/ijds.v21i2.36506 Odovtos - International Journal of Dental Sciences; Vol. 21 No. 2 (2019): Odovtos International Journal of Dental Sciences; 63-72 Odovtos International Journal of Dental Sciences; Vol. 21 Núm. 2 (2019): Odovtos International Journal of Dental Sciences; 63-72 2215-3411 1659-1046 10.15517/ijds.v21i2 eng https://revistas.ucr.ac.cr/index.php/Odontos/article/view/36506/37155 https://revistas.ucr.ac.cr/index.php/Odontos/article/view/36506/37165 https://revistas.ucr.ac.cr/index.php/Odontos/article/view/36506/37986